大学英语词汇短语释义解析及例句 stress corrosion cracking
释义:
stress corrosion cracking 应力腐蚀开裂:一种金属材料在受到应力和腐蚀环境的共同作用下发生的开裂现象
例句:
Stress Corrosion cracking (SCC) is a form of environmental assisted cracking.
应力腐蚀开裂(SCC)是环境辅助开裂的一种形式。
Stress corrosion cracking in which the cracking occurs along grain boundaries.
沿着晶界发生的应力腐蚀开裂。
The results show that the cracking of the pipe is a kind of stress corrosion cracking.
分析结果表明,高压油管的开裂是应力腐蚀开裂造成的。
Stress corrosion cracking problem of concrete beams with crack is studied in this paper.
本文研究了带裂纹混凝土梁的应力腐蚀断裂问题。
The role of hydrogen embrittlement in stress corrosion cracking has also been discussed.
文中还对氢脆在应力腐蚀开裂中的作用进行了讨论。
The results show that evaporator failure was a result of typical stress corrosion cracking.
结果表明,该蒸发釜的失效为典型的应力腐蚀破坏。
The stress corrosion cracking of metastable austenitic stainless steel has been investigated.
研究了亚稳态奥氏体不锈钢的应力腐蚀开裂。
The results show that the fibre orientation affects on the stress corrosion cracking of GRP seriously.
结果表明,纤维取向对玻璃纤维增强塑料的应力腐蚀行为有很大影响。
The stress corrosion cracking (SCC) behaviour of low alloy steel in nitrate aqueous solution was investigated.
研究了低合金钢-硝酸盐溶液体系的应力腐蚀行为。
It was concluded that the cl ion in the oil glue resulted in stress corrosion cracking of the pure copper tube.
结果表明,紫铜管渗漏系腐蚀引发裂纹所致,而涂在铜管表面的油胶中的氯离子是引起紫铜管应力腐蚀开裂的主要因素。
There are reactor coolant system weld issues, they're used and they're getting primary water stress corrosion cracking.
还有反应堆冷却剂系统焊接问题,它们使用了并且得到原生水,应力腐蚀裂痕。
Accidents of liquid ammonia equipment used in petrochemical industry happen mostly due to stress corrosion cracking.
石油化工用液氨设备事故多数源自液氨应力腐蚀开裂。
The results showed that it was chlorine ion that resulted in transgranular stress corrosion cracking in brass tubes.
结果表明,黄铜管的开裂为氯离子引起的穿晶应力腐蚀开裂;
Through-thickness cracking also can lead to fatigue or stress corrosion cracking of the base metal beneath the plating.
还会形成穿透型裂纹,造成镀层下本体金属的疲劳或应力腐蚀裂纹。